摘要 Thestarch/D,L-lactidegraftcopolymersweresynthesizedbyreactingD,L-lactidewithcornstarchinN,N-dimethylacetamide(DMAM)inthepresenceoftriethylamine(NEt3)andanhydrouslithiumchloride.TheeffectofreactiontimeandthemolarratioofD,L-lactidetoglucosestructuralunitofstarchonmonomerconversion(C%),graft(G%)andgraftefficiency(GE%)werestudied,TheC%,G%andGE%couldapproach37.3%179.7%and68.0%,respectivelywhenthemolarratioofD,L-lactidetoglucosestructuralunitofstarchis10:1andthegraftcopolymerizationwascarriedoutat80-85℃for4hrundernitrogenatmosphere.TheFouriertransformsinfra-red(FTIR)spectroscopy.differentialscanningcalorimetry(DSC)andX_raydiffraction(XRD)spectroscopywereusedinordertocharacterizethegraftcopolymers.FTIRspectrashowthatabsorptionbandat1740cm^-1confirmedtheformationofesterbond,indicatingthestarch/D,L-lactidegraftcopolymerswereproduced,theDSCcharacteristicresultsshowthemeltingtemperatureofthegraftcopolymerwereelevatedslightlyasthemolarratioofD,L-lactidetoglucosestructuralunitsofstarchincreasedandtheX-raydiffractionspectrashowthesynthesizedgraftcopolymerswereamorphous.Thedegradabilityofgraftcopolymerwastestedwiththeaidofacid,alkaliandmicrobesuchasbacillussubtilisandstaphylococcusaureus.Theresultsofwaterrsistanceshowthegraftcopolymerproducedcanbeusedasacomponentofimpermeablecoatingforcardboard.
机构地区 不详
出版日期 2000年02月12日(中国期刊网平台首次上网日期,不代表论文的发表时间)
  • 相关文献