Aim:Tostudythestrengthandmicrostructureoftrace-Ti-bearingstracturesteel.MaterialsandMethods:ThestrengthandmicrostructureofthetraceTibearingstructuresteelwerestudiedbytwokindsofcontrolledcoolingsimulationtestingresultsinthefirststagecoolingandthelaststagecoolingafterhotpressdeformationinthetrace-Ti-bearingstructuresteel.Results:Itshowedthattheferritegrainsize,therelativecontributionoftheinvolvedstrengthandthemechanicalstrengthwereinfluencedmoreorlessbydifferentcoolingrates.Boththerefinementofferritegrainandtheincreaseofmechanicalstrengthcouldbeobtainedbytheproperdecreaseofwatercoolinginterruptiontemperature(WTI)andcoilingtemperature(CT)inthefirststagecoolingortheproperincreaseofwatercoolingbeginningtemperature(WTB)andproperdecreaseofcoilingtemperature(CT)inthelaststagecooling.Conclusion:Thestrength,theferritegrainrefinementandtheyieldtensileratiointhefirststagecoolingprocessaremuchbetterthanthoseinthelaststagecoolingprocess.